X100CrMoV5 Cold Work Steel

Ptool steel1.2363 · X100CrMoV5 · A2Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Hardness
58-62 HRC (templado)
Higher than 92% of the catalogue
Machinability
Difficult · 28
Higher than 24% of its family
Density
7.75 g/cm³
Higher than 47% of the catalogue
EN 1.2363Designación X100CrMoV5DIN X100CrMoV5-1AISI/SAE A2UNS T30102JIS SKD12ASTM A681 A2AFNOR Z100CDV5 / X100CrMoV5BS BA2 / BS 4659 BA2GB/T Cr5Mo1VGOST Kh12M (aprox.)ISO 4957 X100CrMoV5Alias Z100CDV5Alias air hardening tool steel
See recommended Vc and feed →

Indicative chemical composition (%)

C 0.95-1.05Si 0.10-0.40Mn 0.40-0.70P ≤0.030S ≤0.030Cr 4.75-5.50Mo 0.90-1.40V 0.15-0.50

Mechanical properties

Elastic modulus (E)

210 GPa

Shear modulus (G)

80.8 GPa

Thermal and electrical properties

Thermal conductivity

22 W/m·K

Thermal expansion

11 µm/m·K

electrical resistivity

0.4 µΩ·m

Workshop behavior

Weldability

Not recommended

Corrosion resistance

Low

Fatigue resistance

High hardness favors fatigue resistance in contact

But is fragile upon impact

Impact resistance

Low in temperate state

Handle with care, risk of brittle fracture

Magnetic?

Yes

Heat treatable

Yes

Vc on the lathe

112–179 m/min

Carbide, medium cut

Vc in milling

90–157 m/min

Carbide, medium cut

Achievable finish (Ra)

0.4–1.6µm

Better with grinding after quenching

See recommended Vc and feed →

Recommended coolant

Whole rough cutting oil

High pressure emulsion in grinding

Chip control

Short brittle chips when hardened

Continuous when annealed

Typical uses

  • Cutting dies and precision punches
  • Air hardening tooling with low deformation

Machining notes and operator tips

Air-hardens with very little deformation, ideal for tight geometry tooling.

  • Always machine in the annealed (soft) condition; hardening comes afterwards, leaving stock for grinding.
  • Avoid stopping the tool in the cut while the part is hot: it can cause unwanted local hardening.
  • For fine features on an already hardened part, consider EDM (wire or sinker) before milling.

Calculate weight and cost of raw bar

Estimated weight

2.435 kg

Sources

  • Standard: EN ISO 4957:2018 · X100CrMoV5
  • Standard: ASTM A681 · A2
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · T30102
  • Standard: ISO 513:2012 · P
  • Manufacturer's official website: Sandvik Coromant MC codes · P3
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps