Skip to content
Back to Cutting parameters calculator

H13 / 1.2344 tool steel speeds and feeds

H13 tool steel (1.2344, X40CrMoV5-1) in the annealed condition is turned at 130-200 m/min (about 425-655 SFM) with 0.22 mm/rev using coated carbide, milled at 110-180 m/min with 0.08 mm/tooth and drilled at 91-150 m/min with 0.12 mm/rev. It is the steel of aluminum die casting dies, forging dies and extrusion tooling: it arrives annealed at around 230 HB and works at 44-52 HRC after hardening.

Designation
EN X40CrMoV5-1 / 1.2344 · AISI H13
Hardness
230 HB (annealed)
ISO group
Steel (P)
Turning Vc
130–200 m/min

Which operation are you machining?

Recommended speeds and feeds

Turning

130–200 m/min

0.22 mm/rev

130-200 m/min at 0.22 mm/rev annealed with a coated steel grade. Hardened (44-52 HRC), hard turning with CBN or carbide for hard materials, light depth of cut and around 80-150 m/min.

Milling

110–180 m/min

0.08 mm/tooth

110-180 m/min at 0.08 mm/tooth annealed. Hardened, hard milling with coated carbide, small radial step and smooth toolpaths: at 48-52 HRC, 80-150 m/min with air blast instead of coolant is common to avoid thermal shock.

Drilling

91–150 m/min

0.12 mm/rev

91-150 m/min and 0.12 mm/rev with a through-coolant carbide drill. Mould cooling channels are long: drill them annealed and, beyond five diameters, program pecks or use a gun drill.

Threading

46–90 m/min

0.12 mm/rev

46-90 m/min for single-point threading with carbide. Mould threads are usually tapped annealed with HSS-E taps at 8-12 m/min; hardened, use a carbide thread mill.

Starting values for coated carbide in medium cutting. Fine-tune them in the calculator for your tool, type of pass and safety margin.

How it behaves when cutting

H13 carries 0.4% carbon, 5% chromium and some molybdenum and vanadium. It has far fewer carbides than D2, so annealed it machines much better: higher speed, less wear and a chip similar to a quenched and tempered alloy steel. It is designed to survive heating and cooling cycles without cracking, which makes it a tough steel: hardened, it mills more safely than other tool steels at the same hardness, which is why it is the typical material for hard milling in mould shops.

Keys to machining it in the shop

Hard milling moulds at 48-52 HRC

With H13 moulds it is common to rough annealed, harden and then finish the cavity by hard milling instead of EDM. To make it work: a rigid machine, short carbide cutters coated for hard materials, a small radial step and constant feed with no sharp entries into corners. Air or MQL usually works better than coolant, because sudden temperature changes crack the edge. Good hard milling greatly reduces polishing afterwards.

H13 vs H11 (1.2343) and ESR grades

H11 / 1.2343 (X37CrMoV5-1) is almost the same but with less vanadium: slightly tougher and slightly less resistant to hot wear. They machine the same. ESR (electroslag remelted) versions have fewer inclusions and a more uniform structure: they polish better and survive more thermal cycles, which is why they are specified for aluminum die casting and polished parts. Same machining parameters, but check the certificate to confirm which version arrived.

Heat treatment and stock allowances

H13 is hardened from about 1,020-1,050 °C, normally in vacuum, and tempered two or three times to working hardness. It distorts little, but large moulds with a lot of material removed do move. The usual route is to rough annealed, stress relieve, semi-finish leaving even stock and finish after hardening. If the mould is nitrided for surface hardness, that is done last, after finishing.

Quick shop tips

  • Rough annealed and finish the cavity by hard milling after hardening.
  • For hard milling, air or MQL is better than flood coolant.
  • Drill all cooling channels before hardening.
  • For polished moulds or aluminum die casting, ask for ESR and check the certificate.
  • Stress relieve between roughing and finishing on large moulds.

Frequently asked questions

Are H13, 1.2344 and X40CrMoV5-1 the same steel?

In practice, yes: X40CrMoV5-1 is the EN name, 1.2344 its material number and H13 the AISI equivalent. They machine and heat treat the same.

How hard is hardened H13?

Between 44 and 52 HRC depending on the temper. Aluminum die casting dies are usually run at 44-48 HRC for toughness; parts that see more wear go harder.

What is the difference between H13 and D2?

H13 is a hot work steel, tough and resistant to temperature changes. D2 is a cold work steel, much harder and more wear resistant but more brittle. Annealed, H13 machines considerably better.

Can hardened H13 be milled?

Yes, and it is standard practice in mould making. With carbide end mills for hard materials, small radial step, a rigid machine and air instead of coolant, 48-52 HRC machines well.

What SFM for annealed H13 with HSS?

Around 18-25 m/min (60-80 SFM) with cobalt HSS-E drills and end mills, with plenty of coolant. For production or large moulds, carbide pays off.

Similar materials

Related apps