Ferritic stainless X6Cr17
PFerritic stainless1.4016 · X6Cr17 · 430Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.
- Strength (Rm)
- 450-630 MPa
- Higher than 51% of the catalogue
- Hardness
- ≤200 HB
- Higher than 45% of the catalogue
- Machinability
- Good · 55
- Higher than 69% of its family
- Density
- 7.7 g/cm³
- Higher than 37% of the catalogue
Indicative chemical composition (%)
Mechanical properties
Elastic limit (Re)
≥260 MPa
Alargamiento (A%)
≥20 %
Thermal and electrical properties
Thermal conductivity
26 W/m·K
Thermal expansion
10.5 µm/m·K
electrical resistivity
0.6 µΩ·m
Workshop behavior
Weldability
Medium
Grain growth in the heat-affected zone
Corrosion resistance
Medium
Nickel free
Fatigue resistance
Moderada-buena
Impact resistance
Less than austenitic and falls when cold
Check the service below zero
Magnetic?
Yes
Heat treatable
No
Vc on the lathe
150–250 m/min
Carbide, medium cut
Vc in milling
150–250 m/min
Carbide, medium cut
Achievable finish (Ra)
0.8–3.2µm
Recommended coolant
Standard soluble emulsion (6-8%)
Less critical than in austenitic
Chip control
Shorter chip than austenitic
With less tendency to tangle
Typical uses
- Household appliances
- Cutlery
- Paneles decorativos
Machining notes and operator tips
It machines better than austenitics; less tough and with less strain hardening.
- Hardens less by deformation than austenitic: you can be somewhat more aggressive with the Vc.
- Its thermal expansion is low (≈10.5 µm/m·K, like a carbon steel): it distorts less from heat than an austenitic grade, though steady coolant is still advisable.
- Avoid long periods at low spindle speed: they promote a built-up edge, just as in austenitic grades.
Calculate weight and cost of raw bar
Estimated weight
2.419 kg
Sources
- Standard: EN 10088-3:2014 · X6Cr17 (1.4016)
- Standard: ISO 15510 · X6Cr17
- Standard: ASTM A240 · 430
- Standard: ASTM A276 · 430
- Standard: ASTM A176 · 430
- Standard: UNS (SAE HS-1086 / ASTM DS-56) · S43000
- Standard: ISO 513:2012 · P
- Manufacturer's official website: Sandvik Coromant MC codes · P5
- Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz
Materials in the same family
Related apps
Hardness converter
Converts shop hardness scales: HRC, HRB, HRA, HRD, superficial N/T, Brinell, Vickers, Knoop, Shore HS and Rm, with a separate table for each material family. It also works out hardness from the indentation and warns you when the test is not valid.
Cutting parameters calculator
Cutting speed (Vc), rpm, feed and theoretical surface finish for turning, milling, drilling and threading by material and tool. A starting point.
Machining quote
Instant machining quote: material, machine time, setup per batch, secondary operations and margin. Free, no sign-up.