Ferritic stainless X6CrMo17-1

PFerritic stainless1.4113 · X6CrMo17-1 · 434Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
480-670 MPa
Higher than 54% of the catalogue
Machinability
Medium · 52
Higher than 68% of its family
Density
7.7 g/cm³
Higher than 37% of the catalogue
EN 1.4113Designación X6CrMo17-1DIN X6CrMo17-1AISI/SAE 434UNS S43400JIS SUS434ASTM A240 434 / A276 434AFNOR Z8CD17-01 / Z7CD17-01BS 434S17 / 434S19GB/T 10Cr17Mo / 1Cr17MoISO 15510 X6CrMo17-1Alias molybdenum ferritic stainless
See recommended Vc and feed →

Indicative chemical composition (%)

C ≤0.12Si ≤1.00Mn ≤1.00P ≤0.040S ≤0.030Cr 16.0-18.0Mo 0.90-1.40

Mechanical properties

Elastic limit (Re)

≥310 MPa

Alargamiento (A%)

≥18 %

Thermal and electrical properties

Thermal conductivity

25 W/m·K

Thermal expansion

10.5 µm/m·K

electrical resistivity

0.6 µΩ·m

Workshop behavior

Weldability

Medium

Corrosion resistance

Better than 430 thanks to the molybdenum

Fatigue resistance

Moderada-buena

Impact resistance

Less than austenitic and falls when cold

Check the service below zero

Magnetic?

Yes

Heat treatable

No

Vc on the lathe

142–236 m/min

Carbide, medium cut

Vc in milling

142–236 m/min

Carbide, medium cut

Achievable finish (Ra)

0.8–3.2µm

See recommended Vc and feed →

Recommended coolant

Standard soluble emulsion (6-8%)

Less critical than in austenitic

Chip control

Shorter chip than austenitic

With less tendency to tangle

Typical uses

  • Automotive moldings
  • Componentes expuestos a sales de deshielo

Machining notes and operator tips

Like 430 but with better resistance to pitting due to the added Mo.

  • Hardens less by deformation than austenitic: you can be somewhat more aggressive with the Vc.
  • Its thermal expansion is low (≈10.5 µm/m·K, like a carbon steel): it distorts less from heat than an austenitic grade, though steady coolant is still advisable.
  • Avoid long periods at low spindle speed: they promote a built-up edge, just as in austenitic grades.

Calculate weight and cost of raw bar

Estimated weight

2.419 kg

Sources

  • Standard: EN 10088-3:2014 · X6CrMo17-1 (1.4113)
  • Standard: ISO 15510 · X6CrMo17-1
  • Standard: ASTM A240 · 434
  • Standard: ASTM A276 · 434
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · S43400
  • Standard: ISO 513:2012 · P
  • Manufacturer's official website: Sandvik Coromant MC codes · P5
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family