EN AW-2007 free-cutting aluminium

NAluminiumEN AW-2007 · AlCu4PbMgMn · 2007 (aprox.)Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
330-420 MPa
Higher than 32% of the catalogue
Hardness
95-110 HB
Higher than 21% of the catalogue
Machinability
Excellent · 100
Higher than 89% of its family
Density
2.85 g/cm³
Higher than 23% of the catalogue
EN EN AW-2007Designación AlCu4PbMgMnAISI/SAE 2007 (aprox.)UNS A92007JIS A2007ASTM B211 2007 (aprox.)AFNOR AU4PbBS 2007ISO 209 AlCu4PbMgMnAlias free machining aluminiumAlias aluminio decoletaje
See recommended Vc and feed →

Indicative chemical composition (%)

Al restoCu 3.3-4.6Pb 0.8-1.5Mg 0.4-1.8Mn 0.50-1.00Fe ≤0.80Si ≤0.80Zn ≤0.80Ti ≤0.20Bi ≤0.20Sn ≤0.20Ni ≤0.20Cr ≤0.10

Mechanical properties

Elastic limit (Re)

≥250 MPa

Alargamiento (A%)

≥10 %

Thermal and electrical properties

Thermal conductivity

150 W/m·K

Thermal expansion

23 µm/m·K

electrical resistivity

0.05 µΩ·m

Workshop behavior

Weldability

Poor

Added lead

Corrosion resistance

Medium

Fatigue resistance

It has no true fatigue limit

Refers to 5×10⁸ cycles, ≈30-40% of Rm

Impact resistance

Good

Without ductile-brittle transition at low temperature

Magnetic?

No

Heat treatable

Yes

Vc on the lathe

571–1429 m/min

Carbide, medium cut

Vc in milling

357–857 m/min

Carbide, medium cut

Achievable finish (Ra)

0.4–1.6µm

Mirror finish possible with diamond tool

See recommended Vc and feed →

Recommended coolant

Soluble emulsion or air

In threading, pure mineral oil. Avoid chlorinated coolants

Chip control

Long, continuous chip (ductile)

Easy cutting alloys (2011) give short chips

Typical uses

  • High production aluminum turning parts
  • Conectores
  • Racores

Machining notes and operator tips

Reference for "free-cutting" aluminium; short chip and a good finish even at high Vc.

  • Use a very sharp edge and a positive rake angle (12-20°) to avoid edge growth.
  • Clear the chips with air or high-pressure coolant; long chips can tangle and mark the part.
  • In high Si casting alloys, it uses polycrystalline diamond (PCD) inserts in production.

Calculate weight and cost of raw bar

Estimated weight

0.895 kg

Sources

  • Standard: EN 573-3 · EN AW-2007
  • Standard: ISO 209 · AlCu4PbMgMn
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · A92007
  • Standard: ISO 513:2012 · N
  • Manufacturer's official website: Sandvik Coromant MC codes · N1
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family