Aluminum profiles EN AW-6060

NAluminiumEN AW-6060 · AlMgSi · 6060Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
150-220 (T5/T6) MPa
Higher than 13% of the catalogue
Hardness
60-75 HB
Higher than 7% of the catalogue
Machinability
Good · 75
Higher than 79% of its family
Density
2.7 g/cm³
Higher than 16% of the catalogue
EN EN AW-6060Designación AlMgSiAISI/SAE 6060UNS A96060UNE L-3441JIS A6060 / A6060SASTM B221 6060AFNOR AGS / A-GSBS 6060GB/T 6060GOST AD31 (aprox.)ISO 209 AlMgSiAlias AA6060Alias L3441Alias AGSAlias extrusion aluminumAlias aluminum profiles
See recommended Vc and feed →

Indicative chemical composition (%)

Al restoMg 0.35-0.60Si 0.30-0.60Fe 0.10-0.30Mn ≤0.10Cu ≤0.10Zn ≤0.15Ti ≤0.10Cr ≤0.05

Mechanical properties

Elastic limit (Re)

≥120 MPa

Alargamiento (A%)

≥8 %

Thermal and electrical properties

Thermal conductivity

200 W/m·K

Thermal expansion

23 µm/m·K

electrical resistivity

0.03 µΩ·m

Workshop behavior

Weldability

Good

Corrosion resistance

Excellent

Fatigue resistance

It has no true fatigue limit

Refers to 5×10⁸ cycles, ≈30-40% of Rm

Impact resistance

Good

Without ductile-brittle transition at low temperature

Magnetic?

No

Heat treatable

Yes

Vc on the lathe

429–1071 m/min

Carbide, medium cut

Vc in milling

268–643 m/min

Carbide, medium cut

Achievable finish (Ra)

0.4–1.6µm

Mirror finish possible with diamond tool

See recommended Vc and feed →

Recommended coolant

Soluble emulsion or air

In threading, pure mineral oil. Avoid chlorinated coolants

Chip control

Long, continuous chip (ductile)

Easy cutting alloys (2011) give short chips

Typical uses

  • Perfiles extruidos de arquitectura
  • Aluminum carpentry

Machining notes and operator tips

Very easy to machine; typical profile from a commercial catalog, not a solid bar.

  • Use a very sharp edge and a positive rake angle (12-20°) to avoid edge growth.
  • Clear the chips with air or high-pressure coolant; long chips can tangle and mark the part.
  • In high Si casting alloys, it uses polycrystalline diamond (PCD) inserts in production.

Calculate weight and cost of raw bar

Estimated weight

0.848 kg

Sources

  • Standard: EN 573-3 · EN AW-6060
  • Standard: ISO 209 · AlMgSi
  • Standard: ASTM B221 · 6060
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · A96060
  • Standard: ISO 513:2012 · N
  • Manufacturer's official website: Sandvik Coromant MC codes · N1
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps