Structural steel ASTM A36

PCarbon steel1.0038 (aprox.) · S235JR (aprox.) · A36Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
400-550 MPa
Higher than 45% of the catalogue
Hardness
120-160 HB
Higher than 30% of the catalogue
Machinability
Good · 62
Higher than 86% of its family
Density
7.85 g/cm³
Higher than 53% of the catalogue
EN 1.0038 (aprox.)Designación S235JR (aprox.)AISI/SAE A36UNS K02600UNE F.111 (aprox.)ASTM A36 / A36MAFNOR E24-2 (aprox.)BS 4360 40A (aprox.)GB/T Q235B (aprox.)GOST St3sp (aprox.)ISO 630 S235JR (aprox.)Alias ASTM A36Alias SA-36Alias structural steelAlias acero estructural americanoAlias carbon structural steel
See recommended Vc and feed →

Indicative chemical composition (%)

C ≤0.26Si 0.15-0.40Mn ≤1.35P ≤0.040S ≤0.050

Mechanical properties

Elastic limit (Re)

≥250 MPa

Alargamiento (A%)

≥20 %

Elastic modulus (E)

200 GPa

Shear modulus (G)

76.9 GPa

Thermal and electrical properties

melting point

~1425-1540 °C

Thermal conductivity

51 W/m·K

Thermal expansion

12 µm/m·K

electrical resistivity

0.17 µΩ·m

Workshop behavior

Weldability

Excellent

Corrosion resistance

Low

Fatigue resistance

Good

Indicative fatigue limit ≈45% of Rm in rotary flexion

Impact resistance

Good toughness at room temperature

Check the service in extreme cold

Magnetic?

Yes

Heat treatable

No

Vc on the lathe

203–316 m/min

Carbide, medium cut

Vc in milling

203–316 m/min

Carbide, medium cut

Achievable finish (Ra)

0.8–3.2µm

See recommended Vc and feed →

Recommended coolant

Soluble emulsion (taladrin) 5-8%

Whole oil in threading or broaching

Chip control

Continuous spiral chips

Use a chipbreaker when roughing to avoid tangles

Typical uses

  • Metallic and welded structure in American standard
  • Vigas
  • Placas base

Machining notes and operator tips

Reference American structural steel; in strength it sits between the European S235JR and S275JR.

  • Use inserts with chipbreakers in roughing to avoid long chips getting caught in the workpiece or spindle.
  • In roughing, it prioritizes high pass depth with moderate feed; In finishing, Vc increases and the feed rate decreases.
  • If a buildup edge appears in very fine finishing passes, raise the Vc slightly instead of lowering it.

Calculate weight and cost of raw bar

Estimated weight

2.466 kg

Sources

  • Standard: ASTM A36
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · K02600
  • Standard: ISO 513:2012 · P
  • Manufacturer's official website: Sandvik Coromant MC codes · P1
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps