Skip to content
Back to Materials Catalog

Structural steel S355JR

PCarbon steel1.0045 · S355JR · A572 Gr.50 (aprox.)Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
470-630 MPa
Higher than 52% of the catalogue
Hardness
140-180 HB
Higher than 37% of the catalogue
Machinability
Good · 60
Higher than 82% of its family
Density
7.85 g/cm³
Higher than 53% of the catalogue
EN 1.0045Designación S355JRDIN St52-3AISI/SAE A572 Gr.50 (aprox.)UNE AE 355 BJIS SM490ASTM A572 Gr.50 / A709 Gr.50AFNOR E36-2 / NF A35-501 S355JRBS 4360 50B / BS EN 10025 S355JRGB/T Q355B / Q345BGOST 17G1S / 09G2SISO 630 S355JRAlias S355Alias St52Alias AE355BAlias S355JRG2Alias high strength structural steel
See recommended Vc and feed →

Indicative chemical composition (%)

C ≤0.24Si ≤0.55Mn ≤1.60P ≤0.035S ≤0.035N ≤0.012Cu ≤0.55

Mechanical properties

Elastic limit (Re)

≥355 MPa

Alargamiento (A%)

≥20 %

Elastic modulus (E)

210 GPa

Shear modulus (G)

80.8 GPa

Thermal and electrical properties

melting point

~1450 °C

Thermal conductivity

50 W/m·K

Thermal expansion

12 µm/m·K

electrical resistivity

0.17 µΩ·m

Workshop behavior

Weldability

Good

Corrosion resistance

Low

Fatigue resistance

Good

Indicative fatigue limit ≈45% of Rm in rotary flexion

Impact resistance

Good toughness at room temperature

Check the service in extreme cold

Magnetic?

Yes

Heat treatable

No

Vc on the lathe

196–305 m/min

Carbide, medium cut

Vc in milling

196–305 m/min

Carbide, medium cut

Achievable finish (Ra)

0.8–3.2µm

See recommended Vc and feed →

Recommended coolant

Soluble emulsion (taladrin) 5-8%

Whole oil in threading or broaching

Chip control

Continuous spiral chips

Use a chipbreaker when roughing to avoid tangles

Typical uses

  • Estructura soldada de mayor exigencia
  • Bastidores
  • Machine chassis

Machining notes and operator tips

Similar to S235JR but more resistant; slightly harder to machine.

  • Use inserts with chipbreakers in roughing to avoid long chips getting caught in the workpiece or spindle.
  • In roughing, it prioritizes high pass depth with moderate feed; In finishing, Vc increases and the feed rate decreases.
  • If a buildup edge appears in very fine finishing passes, raise the Vc slightly instead of lowering it.

Calculate weight and cost of raw bar

Estimated weight

2.466 kg

Sources

  • Standard: EN 10025-2:2019 · S355JR
  • Standard: ISO 630 · S355JR
  • Standard: ASTM A572 · Gr.50
  • Standard: ASTM A709 · Gr.50
  • Standard: ISO 513:2012 · P
  • Manufacturer's official website: Sandvik Coromant MC codes · P1
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps