Skip to content
Back to Materials Catalog

High-carbon steel C60

PCarbon steel1.0601 · C60 · 1060Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
770-920 MPa
Higher than 75% of the catalogue
Hardness
220-250 HB
Higher than 62% of the catalogue
Machinability
Medium · 45
Higher than 54% of its family
Density
7.85 g/cm³
Higher than 53% of the catalogue
EN 1.0601Designación C60DIN Ck60AISI/SAE 1060UNS G10600UNE F.116JIS S58CAFNOR XC60 / XC60H1BS 080A62 / 080A57GB/T 60GOST 60ISO 683-1 C60EAlias F116Alias C60EAlias C60RAlias high carbon steel
See recommended Vc and feed →

Indicative chemical composition (%)

C 0.57-0.65Si ≤0.40Mn 0.60-0.90P ≤0.045S ≤0.045

Mechanical properties

Elastic limit (Re)

≥380 MPa

Alargamiento (A%)

≥11 %

Elastic modulus (E)

210 GPa

Shear modulus (G)

80.8 GPa

Thermal and electrical properties

melting point

~1420 °C

Thermal conductivity

46 W/m·K

Thermal expansion

12 µm/m·K

electrical resistivity

0.17 µΩ·m

Workshop behavior

Weldability

Difficult

High carbon, risk of cracks

Corrosion resistance

Low

Fatigue resistance

Good

Indicative fatigue limit ≈45% of Rm in rotary flexion

Impact resistance

Good toughness at room temperature

Check the service in extreme cold

Magnetic?

Yes

Heat treatable

Yes

Vc on the lathe

147–229 m/min

Carbide, medium cut

Vc in milling

147–229 m/min

Carbide, medium cut

Achievable finish (Ra)

0.8–3.2µm

See recommended Vc and feed →

Recommended coolant

Soluble emulsion (taladrin) 5-8%

Whole oil in threading or broaching

Chip control

Continuous spiral chips

Use a chipbreaker when roughing to avoid tangles

Typical uses

  • Resortes
  • Discos
  • Parts with high wear resistance

Machining notes and operator tips

More abrasive than C45; reduces Vc and monitors insert wear in roughing.

  • Use inserts with chipbreakers in roughing to avoid long chips getting caught in the workpiece or spindle.
  • In roughing, it prioritizes high pass depth with moderate feed; In finishing, Vc increases and the feed rate decreases.
  • If a buildup edge appears in very fine finishing passes, raise the Vc slightly instead of lowering it.

Calculate weight and cost of raw bar

Estimated weight

2.466 kg

Sources

  • Standard: EN ISO 683-1 · C60
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · G10600
  • Standard: ISO 513:2012 · P
  • Manufacturer's official website: Sandvik Coromant MC codes · P1
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps