Aluminio estructural EN AW-5754
NAluminiumEN AW-5754 · AlMg3 · 5754Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.
- Strength (Rm)
- 190-240 MPa
- Higher than 16% of the catalogue
- Hardness
- 50-75 HB
- Higher than 5% of the catalogue
- Machinability
- Good · 55
- Higher than 0% of its family
- Density
- 2.67 g/cm³
- Higher than 13% of the catalogue
Indicative chemical composition (%)
Mechanical properties
Elastic limit (Re)
≥80 MPa
Alargamiento (A%)
≥12 %
Thermal and electrical properties
Thermal conductivity
134 W/m·K
Thermal expansion
23 µm/m·K
electrical resistivity
0.03 µΩ·m
Workshop behavior
Weldability
Excellent
Corrosion resistance
Muy buena
Fatigue resistance
It has no true fatigue limit
Refers to 5×10⁸ cycles, ≈30-40% of Rm
Impact resistance
Good
Without ductile-brittle transition at low temperature
Magnetic?
No
Heat treatable
No
Vc on the lathe
314–786 m/min
Carbide, medium cut
Vc in milling
196–471 m/min
Carbide, medium cut
Achievable finish (Ra)
0.4–1.6µm
Mirror finish possible with diamond tool
Recommended coolant
Soluble emulsion or air
In threading, pure mineral oil. Avoid chlorinated coolants
Chip control
Long, continuous chip (ductile)
Easy cutting alloys (2011) give short chips
Typical uses
- Automotive sheet metal and bodywork
- Estructuras plegadas de responsabilidad media
Machining notes and operator tips
Widely used in automotive sheet metal due to its good forming/strength/welding ratio.
- Use a very sharp edge and a positive rake angle (12-20°) to avoid edge growth.
- Clear the chips with air or high-pressure coolant; long chips can tangle and mark the part.
- In high Si casting alloys, it uses polycrystalline diamond (PCD) inserts in production.
Calculate weight and cost of raw bar
Estimated weight
0.839 kg
Sources
- Standard: EN 573-3 · EN AW-5754
- Standard: ISO 209 · AlMg3
- Standard: ASTM B209 · 5754
- Standard: ASTM B928 · 5754
- Standard: UNS (SAE HS-1086 / ASTM DS-56) · A95754
- Standard: ISO 513:2012 · N
- Manufacturer's official website: Sandvik Coromant MC codes · N1
- Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz
Materials in the same family
Related apps
Hardness converter
Converts shop hardness scales: HRC, HRB, HRA, HRD, superficial N/T, Brinell, Vickers, Knoop, Shore HS and Rm, with a separate table for each material family. It also works out hardness from the indentation and warns you when the test is not valid.
Cutting parameters calculator
Cutting speed (Vc), rpm, feed and theoretical surface finish for turning, milling, drilling and threading by material and tool. A starting point.
Machining quote
Instant machining quote: material, machine time, setup per batch, secondary operations and margin. Free, no sign-up.