Martensitic stainless X12Cr13
PMartensitic stainless1.4006 · X12Cr13 · 410Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.
- Strength (Rm)
- 540-740 (annealed or quenched and tempered) MPa
- Higher than 64% of the catalogue
- Hardness
- 38-42 HRC as-quenched
- Higher than 79% of the catalogue
- Machinability
- Good · 55
- Higher than 69% of its family
- Density
- 7.7 g/cm³
- Higher than 37% of the catalogue
Indicative chemical composition (%)
Thermal and electrical properties
Thermal conductivity
26 W/m·K
Thermal expansion
10.5 µm/m·K
electrical resistivity
0.55 µΩ·m
Workshop behavior
Weldability
Media
Precalentar
Corrosion resistance
Basic
Soft environments only
Fatigue resistance
Good in the quenched-and-tempered condition
Impact resistance
Moderate
It drops if tempering falls in the temper-embrittlement range
Magnetic?
Yes
Heat treatable
Yes
Vc on the lathe
126–206 m/min
Carbide, medium cut
Vc in milling
126–206 m/min
Carbide, medium cut
Achievable finish (Ra)
0.4–1.6µm
Good finish when hardened and ground
Recommended coolant
High concentration soluble emulsion
In a warm state, low Vc and abundant cooling
Chip control
Short to medium chip
Shorter the harder the material
Typical uses
- Screws and pump shafts
- Low demand steam turbine blades
- Basic cutlery
Machining notes and operator tips
The most common and economical martensitic; Low carbon makes machining easier compared to 420.
- In the hardened condition, lower Vc and take light finishing passes: the material is more abrasive on the edge.
- If you are going to grind after quenching, leave 0.2-0.3 mm of extra thickness in the previous machining.
- Avoid interrupted cuts on hardened parts: it raises the risk of micro-cracks in the insert edge.
Calculate weight and cost of raw bar
Estimated weight
2.419 kg
Sources
- Standard: EN 10088-3:2014 · X12Cr13 (1.4006)
- Standard: ISO 15510 · X12Cr13
- Standard: ASTM A240 · 410
- Standard: ASTM A276 · 410
- Standard: ASTM A182 · F6a
- Standard: SAE AMS 5504 / 5591
- Standard: UNS (SAE HS-1086 / ASTM DS-56) · S41000
- Standard: ISO 513:2012 · P
- Manufacturer's official website: Sandvik Coromant MC codes · P5
- Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz
Materials in the same family
Related apps
Hardness converter
Converts shop hardness scales: HRC, HRB, HRA, HRD, superficial N/T, Brinell, Vickers, Knoop, Shore HS and Rm, with a separate table for each material family. It also works out hardness from the indentation and warns you when the test is not valid.
Cutting parameters calculator
Cutting speed (Vc), rpm, feed and theoretical surface finish for turning, milling, drilling and threading by material and tool. A starting point.
Machining quote
Instant machining quote: material, machine time, setup per batch, secondary operations and margin. Free, no sign-up.