Skip to content
Back to Materials Catalog

X12CrS13 free-cutting martensitic stainless

PMartensitic stainless1.4005 · X12CrS13 · 416Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
520-720 (templado) MPa
Higher than 59% of the catalogue
Hardness
35-42 HRC (templado)
Higher than 77% of the catalogue
Machinability
Excellent · 85
Higher than 97% of its family
Density
7.7 g/cm³
Higher than 37% of the catalogue
EN 1.4005Designación X12CrS13DIN X12CrS13AISI/SAE 416UNS S41600UNE F-3411JIS SUS416AMS 5610ASTM A582 416 / A314 416AFNOR Z13CF13 / Z11CF13BS 416S21 / 416S29GB/T Y1Cr13 / Y3Cr13GOST 12Kh13E (aprox.)ISO 15510 X12CrS13Alias free machining martensitic stainlessAlias martensitic bar turning stainless steel
See recommended Vc and feed →

Indicative chemical composition (%)

C ≤0.15Si ≤1.00Mn ≤1.50P ≤0.060S ≥0.15Cr 12.0-14.0

Thermal and electrical properties

Thermal conductivity

26 W/m·K

Thermal expansion

10.5 µm/m·K

electrical resistivity

0.55 µΩ·m

Workshop behavior

Weldability

Deficient

Added sulfur

Corrosion resistance

Slightly lower than 410 because of the S

Fatigue resistance

Good in the quenched-and-tempered condition

Impact resistance

Moderate

It drops if tempering falls in the temper-embrittlement range

Magnetic?

Yes

Heat treatable

Yes

Vc on the lathe

195–319 m/min

Carbide, medium cut

Vc in milling

195–319 m/min

Carbide, medium cut

Achievable finish (Ra)

0.4–1.6µm

Good finish when hardened and ground

See recommended Vc and feed →

Recommended coolant

High concentration soluble emulsion

In a warm state, low Vc and abundant cooling

Chip control

Short to medium chip

Shorter the harder the material

Typical uses

  • High production lathe parts in martensitic stainless
  • Shafts and valves

Machining notes and operator tips

Reference for machinability among martensitics thanks to the added sulfur.

  • In the hardened condition, lower Vc and take light finishing passes: the material is more abrasive on the edge.
  • If you are going to grind after quenching, leave 0.2-0.3 mm of extra thickness in the previous machining.
  • Avoid interrupted cuts on hardened parts: it raises the risk of micro-cracks in the insert edge.

Calculate weight and cost of raw bar

Estimated weight

2.419 kg

Sources

  • Standard: EN 10088-3:2014 · X12CrS13 (1.4005)
  • Standard: ISO 15510 · X12CrS13
  • Standard: ASTM A582 · 416
  • Standard: ASTM A314 · 416
  • Standard: SAE AMS 5610
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · S41600
  • Standard: ISO 513:2012 · P
  • Manufacturer's official website: Sandvik Coromant MC codes · P5
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps