Martensitic stainless X39Cr13

PMartensitic stainless1.4031 · X39Cr13 · 420B (aprox.)Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Hardness
52-56 HRC (templado)
Higher than 89% of the catalogue
Machinability
Medium · 42
Higher than 54% of its family
Density
7.7 g/cm³
Higher than 37% of the catalogue
EN 1.4031Designación X39Cr13DIN X38Cr13AISI/SAE 420B (aprox.)UNS S42000JIS SUS420J2ASTM A276 420 / A314AFNOR Z40C13 / Z40C14BS 420S45GB/T 40Cr13 / 4Cr13 / 3Cr13GOST 40Kh13ISO 15510 X39Cr13Alias 420BAlias 420J2Alias X40Cr13Alias 3Cr13Alias 4Cr13Alias high carbon cutlery stainless
See recommended Vc and feed →

Indicative chemical composition (%)

C 0.36-0.42Si ≤1.00Mn ≤1.50P ≤0.040S ≤0.015Cr 12.0-14.0

Thermal and electrical properties

Thermal conductivity

25 W/m·K

Thermal expansion

10.5 µm/m·K

electrical resistivity

0.55 µΩ·m

Workshop behavior

Weldability

Not recommended

Corrosion resistance

Medium

Fatigue resistance

Good in the quenched-and-tempered condition

Impact resistance

Moderate

It drops if tempering falls in the temper-embrittlement range

Magnetic?

Yes

Heat treatable

Yes

Vc on the lathe

96–158 m/min

Carbide, medium cut

Vc in milling

96–158 m/min

Carbide, medium cut

Achievable finish (Ra)

0.4–1.6µm

Good finish when hardened and ground

See recommended Vc and feed →

Recommended coolant

High concentration soluble emulsion

In a warm state, low Vc and abundant cooling

Chip control

Short to medium chip

Shorter the harder the material

Typical uses

  • High-end cutlery
  • Components with wear and some corrosion

Machining notes and operator tips

More carbon than standard 420: higher achievable hardness and lower machinability.

  • In the hardened condition, lower Vc and take light finishing passes: the material is more abrasive on the edge.
  • If you are going to grind after quenching, leave 0.2-0.3 mm of extra thickness in the previous machining.
  • Avoid interrupted cuts on hardened parts: it raises the risk of micro-cracks in the insert edge.

Calculate weight and cost of raw bar

Estimated weight

2.419 kg

Sources

  • Standard: EN 10088-3:2014 · X39Cr13 (1.4031)
  • Standard: ISO 15510 · X39Cr13
  • Standard: ASTM A276 · 420
  • Standard: ASTM A314
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · S42000
  • Standard: ISO 513:2012 · P
  • Manufacturer's official website: Sandvik Coromant MC codes · P5
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps