Martensitic stainless X20Cr13
PMartensitic stainless1.4021 · X20Cr13 · 420Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.
- Strength (Rm)
- 650-850 (quenched and tempered) MPa
- Higher than 71% of the catalogue
- Hardness
- 200-250 HB quenched and tempered; 48-52 HRC as-quenched
- Higher than 57% of the catalogue
- Machinability
- Medium · 48
- Higher than 64% of its family
- Density
- 7.7 g/cm³
- Higher than 37% of the catalogue
Indicative chemical composition (%)
Thermal and electrical properties
Thermal conductivity
25 W/m·K
Thermal expansion
10.5 µm/m·K
electrical resistivity
0.55 µΩ·m
Workshop behavior
Weldability
Difficult
Martensitic, requires preheating and post-treatment
Corrosion resistance
Media
Solo en estado pulido/pasivado
Fatigue resistance
Good in the quenched-and-tempered condition
Impact resistance
Moderate
It drops if tempering falls in the temper-embrittlement range
Magnetic?
Yes
Heat treatable
Yes
Vc on the lathe
110–180 m/min
Carbide, medium cut
Vc in milling
110–180 m/min
Carbide, medium cut
Achievable finish (Ra)
0.4–1.6µm
Good finish when hardened and ground
Recommended coolant
High concentration soluble emulsion
In a warm state, low Vc and abundant cooling
Chip control
Short to medium chip
Shorter the harder the material
Typical uses
- Knives
- Surgical instrumentation
- Plastic molds with moderate corrosion resistance
Machining notes and operator tips
Preferably machine in the annealed condition; final quenching raises hardness a lot.
- In the hardened condition, lower Vc and take light finishing passes: the material is more abrasive on the edge.
- If you are going to grind after quenching, leave 0.2-0.3 mm of extra thickness in the previous machining.
- Avoid interrupted cuts on hardened parts: it raises the risk of micro-cracks in the insert edge.
Calculate weight and cost of raw bar
Estimated weight
2.419 kg
Sources
- Standard: EN 10088-3:2014 · X20Cr13 (1.4021)
- Standard: ISO 15510 · X20Cr13
- Standard: ASTM A240 · 420
- Standard: ASTM A276 · 420
- Standard: SAE AMS 5506 / 5621
- Standard: UNS (SAE HS-1086 / ASTM DS-56) · S42000
- Standard: ISO 513:2012 · P
- Manufacturer's official website: Sandvik Coromant MC codes · P5
- Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz
Materials in the same family
Related apps
Hardness converter
Converts shop hardness scales: HRC, HRB, HRA, HRD, superficial N/T, Brinell, Vickers, Knoop, Shore HS and Rm, with a separate table for each material family. It also works out hardness from the indentation and warns you when the test is not valid.
Cutting parameters calculator
Cutting speed (Vc), rpm, feed and theoretical surface finish for turning, milling, drilling and threading by material and tool. A starting point.
Machining quote
Instant machining quote: material, machine time, setup per batch, secondary operations and margin. Free, no sign-up.