Skip to content
Back to Materials Catalog

Martensitic stainless X65Cr14

PMartensitic stainless1.4109 (aprox.) · X70CrMo15 · 440AIndicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Hardness
54-57 HRC (templado)
Higher than 90% of the catalogue
Machinability
Medium · 35
Higher than 33% of its family
Density
7.7 g/cm³
Higher than 37% of the catalogue
EN 1.4109 (aprox.)Designación X70CrMo15DIN X70CrMo15AISI/SAE 440AUNS S44002JIS SUS440AASTM A276 440AAFNOR Z70C15 / Z65C14BS S142 (aprox.)GB/T 68Cr17 / 7Cr17GOST 70Kh14 (aprox.)ISO 15510 X70CrMo15Alias 1.4109Alias 440-AAlias cutlery stainless
See recommended Vc and feed →

Indicative chemical composition (%)

C 0.60-0.75Si ≤1.00Mn ≤1.00P ≤0.040S ≤0.015Cr 16.0-18.0Mo ≤0.75

Thermal and electrical properties

Thermal conductivity

24 W/m·K

Thermal expansion

10.5 µm/m·K

electrical resistivity

0.55 µΩ·m

Workshop behavior

Weldability

Not recommended

Corrosion resistance

Good for being martensitic

Fatigue resistance

Good in the quenched-and-tempered condition

Impact resistance

Moderate

It drops if tempering falls in the temper-embrittlement range

Magnetic?

Yes

Heat treatable

Yes

Vc on the lathe

80–131 m/min

Carbide, medium cut

Vc in milling

80–131 m/min

Carbide, medium cut

Achievable finish (Ra)

0.4–1.6µm

Good finish when hardened and ground

See recommended Vc and feed →

Recommended coolant

High concentration soluble emulsion

In a warm state, low Vc and abundant cooling

Chip control

Short to medium chip

Shorter the harder the material

Typical uses

  • Mid-high range cutlery
  • Instrumental que requiere algo de flexibilidad frente al 440C

Machining notes and operator tips

Less carbon than 440C: somewhat less hard but more tenacious.

  • In the hardened condition, lower Vc and take light finishing passes: the material is more abrasive on the edge.
  • If you are going to grind after quenching, leave 0.2-0.3 mm of extra thickness in the previous machining.
  • Avoid interrupted cuts on hardened parts: it raises the risk of micro-cracks in the insert edge.

Calculate weight and cost of raw bar

Estimated weight

2.419 kg

Sources

  • Standard: ISO 15510 · X70CrMo15
  • Standard: ASTM A276 · 440A
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · S44002
  • Standard: ISO 513:2012 · P
  • Manufacturer's official website: Sandvik Coromant MC codes · P5
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps