Skip to content
Back to Materials Catalog

Incoloy 800 Alloy

SNickel and superalloys1.4876 · X10NiCrAlTi32-21 · UNS N08800Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
520-720 MPa
Higher than 59% of the catalogue
Machinability
Difficult · 25
Higher than 20% of its family
Density
7.94 g/cm³
Higher than 76% of the catalogue
EN 1.4876Designación X10NiCrAlTi32-21AISI/SAE UNS N08800UNS N08800JIS NCF800AMS 5766 / 5871ASTM B163 N08800 / B407 N08800 / B408 N08800 / B409 N08800AFNOR Z8NC33-21BS 3072 NA15 / 3076 NA15GB/T NS111 / NS1101GOST KhN32T (aprox.)ISO 9723 X10NiCrAlTi32-21Alias Incoloy 800Alias Alloy 800Alias 800Alias Nicrofer 3220Alias NS111Alias AMS 5766
Tampering Risk: Fine machining/grinding dust can cause skin sensitization to nickel; use extraction and PPE.
See recommended Vc and feed →

Indicative chemical composition (%)

Ni 30.0-35.0Cr 19.0-23.0Fe ≥39.5C ≤0.10Mn ≤1.50Si ≤1.00Cu ≤0.75Al 0.15-0.60Ti 0.15-0.60S ≤0.015

Mechanical properties

Elastic limit (Re)

≥205 MPa

Alargamiento (A%)

≥30 %

Thermal and electrical properties

Temp. max. of service

1100 °C

Thermal conductivity

11.5 W/m·K

Thermal expansion

13.5 µm/m·K

electrical resistivity

1.15 µΩ·m

Workshop behavior

Weldability

Excellent

Corrosion resistance

Very good at high temperatures

Resistant to carburization

Fatigue resistance

Excellent at high temperature

That is why it is used in turbines

Impact resistance

Good

And retained even at high temperature

Magnetic?

No

Nickel 200 is magnetic (practically pure nickel) and Monel 400 is slightly magnetic.

Heat treatable

No

Vc on the lathe

42–104 m/min

Carbide, medium cut

Vc in milling

52–73 m/min

Carbide, medium cut

Achievable finish (Ra)

1.6–6.3µm

Strain hardening limits fine finishing

See recommended Vc and feed →

Recommended coolant

Abundant high pressure cooling

High concentration coolant or whole oil

Chip control

Continuous, very tough chips that weld to the edge easily

Adhesion

Typical uses

  • Petrochemical reforming and cracking tubes
  • Componentes de horno industrial

Machining notes and operator tips

Less demanding than Ni-Cr-Mo superalloys; It can be treated with similar criteria to difficult austenitic stainless.

  • Change the edge preventively (due to time, not just visible wear); Catastrophic failure is rapid.
  • These softer nickel alloys are machined with sharp, positive carbide; ceramics are kept for roughing superalloys such as 718.
  • Avoid any vibration: strain hardening becomes much worse with unstable cutting.

Calculate weight and cost of raw bar

Estimated weight

2.494 kg

Sources

  • Standard: ISO 9723 · X10NiCrAlTi32-21
  • Standard: ASTM B163 · N08800
  • Standard: ASTM B407 · N08800
  • Standard: ASTM B408 · N08800
  • Standard: SAE AMS 5766 / 5871
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · N08800
  • Standard: ISO 513:2012 · S
  • Manufacturer's official website: Sandvik Coromant MC codes · S1
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps