Inconel 718 Superalloy

SNickel and superalloys2.4668 · NiCr19NbMo · UNS N07718Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
1240-1450 (envejecido) MPa
Higher than 95% of the catalogue
Hardness
36-44 HRC
Higher than 79% of the catalogue
Machinability
Difficult · 12
Higher than 6% of its family
Density
8.19 g/cm³
Higher than 82% of the catalogue
EN 2.4668Designación NiCr19NbMoAISI/SAE UNS N07718UNS N07718AMS 5589 / 5590 / 5596 / 5597 / 5662 / 5663 / 5664 / 5832 / 5383 / 5384ASTM B637 N07718 / B670 N07718 / B983 N07718AFNOR NC19FeNbBS HR8 / HR507GB/T GH4169 / GH169GOST KhN45MVTYuBR (aprox.)ISO 9723 NiCr19Fe19NbMo3Alias Inconel 718Alias Alloy 718Alias IN718Alias 718Alias GH4169Alias GH169Alias Nicrofer 5219 NbAlias Udimet 718Alias AMS 5662Alias AMS 5663Alias AMS 5664Alias AMS 5596Alias AMS 5589Alias aerospace nickel superalloyAlias aeronautical superalloy
Tampering Risk: Fine machining/grinding dust can cause skin sensitization to nickel; use extraction and PPE.
See recommended Vc and feed →

Indicative chemical composition (%)

Ni 50.0-55.0Cr 17.0-21.0Fe restoNb 4.75-5.50Mo 2.80-3.30Ti 0.65-1.15Al 0.20-0.80Co ≤1.00Mn ≤0.35Si ≤0.35C ≤0.08P ≤0.015S ≤0.015B ≤0.006Cu ≤0.30

Mechanical properties

Elastic limit (Re)

≥1035 MPa

Alargamiento (A%)

≥12 %

Thermal and electrical properties

Temp. max. of service

700 °C

Thermal conductivity

11.4 W/m·K

Thermal expansion

13.5 µm/m·K

electrical resistivity

1.15 µΩ·m

Workshop behavior

Weldability

Good

Weldable superalloy, widely used in aerojets

Corrosion resistance

Excelente a alta temperatura

Fatigue resistance

Excellent at high temperature

That is why it is used in turbines

Impact resistance

Good

And retained even at high temperature

Magnetic?

No

Nickel 200 is magnetic (practically pure nickel) and Monel 400 is slightly magnetic.

Heat treatable

Yes

Vc on the lathe

20–50 m/min

Carbide, medium cut

Vc in milling

25–35 m/min

Carbide, medium cut

Achievable finish (Ra)

1.6–6.3µm

Strain hardening limits fine finishing

See recommended Vc and feed →

Recommended coolant

Abundant high pressure cooling

High concentration coolant or whole oil

Chip control

Continuous, very tough chips that weld to the edge easily

Adhesion

Typical uses

  • Turbine discs and blades
  • Aeronautical engine components
  • High temperature fasteners

Machining notes and operator tips

It hardens greatly due to deformation and retains heat on the edge. Very low Vc, ceramic/CBN inserts in production and frequent edge changes.

  • Change the edge preventively (due to time, not just visible wear); Catastrophic failure is rapid.
  • Use ceramic or CBN inserts in production; carbide wears out very quickly in this material.
  • Avoid any vibration: strain hardening becomes much worse with unstable cutting.

Calculate weight and cost of raw bar

Estimated weight

2.573 kg

Sources

  • Standard: ISO 9723 · NiCr19Fe19NbMo3
  • Standard: ASTM B637 · N07718
  • Standard: ASTM B670 · N07718
  • Standard: ASTM B983 · N07718
  • Standard: SAE AMS 5589 / 5590
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · N07718
  • Standard: ISO 513:2012 · S
  • Manufacturer's official website: Sandvik Coromant MC codes · S2
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps