Skip to content
Back to Materials Catalog

Monel Alloy 400

SNickel and superalloys2.4360 · NiCu30Fe · UNS N04400Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
480-680 MPa
Higher than 54% of the catalogue
Machinability
Difficult · 25
Higher than 20% of its family
Density
8.8 g/cm³
Higher than 92% of the catalogue
EN 2.4360Designación NiCu30FeAISI/SAE UNS N04400UNS N04400JIS NW4400AMS 4544 / 4574 / 4675 / 4730 / 4731ASTM B127 N04400 / B164 N04400 / B165 N04400AFNOR NU-30 / NU30BS NA13 / 3072 NA13GB/T NCu30GOST NMZhMts28-2.5-1.5 (aprox.)ISO 9723 NiCu30FeAlias Monel 400Alias Monel-400Alias MonelAlias Nicorros 400Alias Nickel Alloy 400Alias AMS 4544Alias AMS 4574Alias AMS 4675
Tampering Risk: Fine machining/grinding dust can cause skin sensitization to nickel; use extraction and PPE.
See recommended Vc and feed →

Indicative chemical composition (%)

Ni ≥63.0Cu 28.0-34.0Fe ≤2.50Mn ≤2.00C ≤0.30Si ≤0.50S ≤0.024

Mechanical properties

Elastic limit (Re)

≥170 MPa

Alargamiento (A%)

≥35 %

Thermal and electrical properties

Thermal conductivity

21.8 W/m·K

Thermal expansion

13.5 µm/m·K

electrical resistivity

0.55 µΩ·m

Workshop behavior

Weldability

Good

Corrosion resistance

Excellent in seawater and hydrofluoric acid

Fatigue resistance

Excellent at high temperature

That is why it is used in turbines

Impact resistance

Good

And retained even at high temperature

Magnetic?

Parcial

Nickel 200 is magnetic (practically pure nickel) and Monel 400 is slightly magnetic.

Heat treatable

No

Vc on the lathe

42–104 m/min

Carbide, medium cut

Vc in milling

52–73 m/min

Carbide, medium cut

Achievable finish (Ra)

1.6–6.3µm

Strain hardening limits fine finishing

See recommended Vc and feed →

Recommended coolant

Abundant high pressure cooling

High concentration coolant or whole oil

Chip control

Continuous, very tough chips that weld to the edge easily

Adhesion

Typical uses

  • Marine shafts and propellers
  • Seawater valves
  • Chemical instrumentation

Machining notes and operator tips

Less demanding than Inconel but still strain hardening; Avoid too light finishing passes.

  • Change the edge preventively (due to time, not just visible wear); Catastrophic failure is rapid.
  • These softer nickel alloys are machined with sharp, positive carbide; ceramics are kept for roughing superalloys such as 718.
  • Avoid any vibration: strain hardening becomes much worse with unstable cutting.

Calculate weight and cost of raw bar

Estimated weight

2.765 kg

Sources

  • Standard: ISO 9723 · NiCu30Fe
  • Standard: ASTM B127 · N04400
  • Standard: ASTM B164 · N04400
  • Standard: ASTM B165 · N04400
  • Standard: SAE AMS 4544 / 4574
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · N04400
  • Standard: ISO 513:2012 · S
  • Manufacturer's official website: Sandvik Coromant MC codes · S2
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps