SNickel and superalloys2.4816 · NiCr15Fe · UNS N06600Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
550-750 MPa
Higher than 65% of the catalogue
Machinability
Difficult · 15
Higher than 11% of its family
Density
8.47 g/cm³
Higher than 90% of the catalogue
EN 2.4816Designación NiCr15FeAISI/SAE UNS N06600UNS N06600JIS NCF600AMS 5540 / 5580 / 5665 / 5687ASTM B166 N06600 / B167 N06600 / B168 N06600AFNOR NC15FeBS NA14 / HR203GB/T NS312 / NCr15FeISO 9723 NiCr15FeAlias Inconel 600Alias Alloy 600Alias IN600Alias 600Alias Nicrofer 7216Alias NS312Alias AMS 5540Alias AMS 5665Alias AMS 5687
Tampering Risk: Fine machining/grinding dust can cause skin sensitization to nickel; use extraction and PPE.
See recommended Vc and feed →

Indicative chemical composition (%)

Ni ≥72.0Cr 14.0-17.0Fe 6.00-10.0Mn ≤1.00C ≤0.15Si ≤0.50S ≤0.015Cu ≤0.50

Mechanical properties

Elastic limit (Re)

≥240 MPa

Alargamiento (A%)

≥30 %

Thermal and electrical properties

Temp. max. of service

1150 °C

Thermal conductivity

14.9 W/m·K

Thermal expansion

13.5 µm/m·K

electrical resistivity

1.15 µΩ·m

Workshop behavior

Weldability

Excellent

Corrosion resistance

Excellent at high temperature and in oxidising/reducing environments

Fatigue resistance

Excellent at high temperature

That is why it is used in turbines

Impact resistance

Good

And retained even at high temperature

Magnetic?

No

Nickel 200 is magnetic (practically pure nickel) and Monel 400 is slightly magnetic.

Heat treatable

No

Vc on the lathe

25–63 m/min

Carbide, medium cut

Vc in milling

31–44 m/min

Carbide, medium cut

Achievable finish (Ra)

1.6–6.3µm

Strain hardening limits fine finishing

See recommended Vc and feed →

Recommended coolant

Abundant high pressure cooling

High concentration coolant or whole oil

Chip control

Continuous, very tough chips that weld to the edge easily

Adhesion

Typical uses

  • Furnace components and heat treatment
  • Nuclear and petrochemical exchanger tubes

Machining notes and operator tips

No precipitation hardening (unlike 718); It remains abrasive and has low thermal conductivity.

  • Change the edge preventively (due to time, not just visible wear); Catastrophic failure is rapid.
  • Use ceramic or CBN inserts in production; carbide wears out very quickly in this material.
  • Avoid any vibration: strain hardening becomes much worse with unstable cutting.

Calculate weight and cost of raw bar

Estimated weight

2.661 kg

Sources

  • Standard: ISO 9723 · NiCr15Fe
  • Standard: ASTM B166 · N06600
  • Standard: ASTM B167 · N06600
  • Standard: ASTM B168 · N06600
  • Standard: SAE AMS 5540 / 5580
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · N06600
  • Standard: ISO 513:2012 · S
  • Manufacturer's official website: Sandvik Coromant MC codes · S2
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz