Titanio beta Ti-10V-2Fe-3Al

STitaniumTiV10Fe2Al3Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
1170-1250 (tratado STA) MPa
Higher than 93% of the catalogue
Machinability
Difficult · 18
Higher than 15% of its family
Density
4.65 g/cm³
Higher than 27% of the catalogue
Designación TiV10Fe2Al3UNS R56410AMS 4984 / 4986 / 4987AFNOR T-V10Fe2Al3 (aprox.)GB/T TB6 / TB6-1GOST VT35 (aprox.)Alias Ti-10-2-3Alias Ti-10V-2Fe-3AlAlias TB6Alias AMS 4984Alias AMS 4986Alias AMS 4987Alias beta titaniumAlias titanium landing gear alloy
See recommended Vc and feed →

Indicative chemical composition (%)

Ti restoV 9.00-11.0Fe 1.60-2.20Al 2.60-3.40O ≤0.13C ≤0.05N ≤0.05H ≤0.015

Mechanical properties

Elastic limit (Re)

≥1100 MPa

Alargamiento (A%)

≥6 %

Thermal and electrical properties

Thermal conductivity

7.65 W/m·K

Thermal expansion

9 µm/m·K

electrical resistivity

1.7 µΩ·m

Workshop behavior

Weldability

Medium

Corrosion resistance

Excellent

Fatigue resistance

Very good fatigue/weight ratio

Sensitive to surface finish

Impact resistance

Good

And retained at low temperature

Magnetic?

No

Heat treatable

Yes

Vc on the lathe

36–72 m/min

Carbide, medium cut

Vc in milling

36–72 m/min

Carbide, medium cut

Achievable finish (Ra)

0.8–3.2µm

Built-up edge limits very fine finishes

See recommended Vc and feed →

Recommended coolant

Abundant high pressure cooling

Whole oil or highly concentrated emulsion. Avoid chlorinated refrigerants (stress corrosion)

Chip control

Short and very hot chip, concentrated on the edge

Risk of ignition if fine buildup

Typical uses

  • Componentes forjados de tren de aterrizaje de alta resistencia
  • Critical commercial aviation structural parts

Machining notes and operator tips

Very high strength beta alloy; machine in solution condition (softer) before aging whenever the geometry allows.

  • Never stop feeding with the tool in contact; the heat concentrates and damages the edge and the part.
  • Do a single finishing pass whenever you can: going over hardens the already machined surface.
  • Keep the pass depth above the hardened layer thickness of the previous pass.

Calculate weight and cost of raw bar

Estimated weight

1.461 kg

Sources

  • Standard: SAE AMS 4984 / 4986
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · R56410
  • Standard: ISO 513:2012 · S
  • Manufacturer's official website: Sandvik Coromant MC codes · S4
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps