Palladium-alloyed titanium Grade 7

STitanium3.7235 · TiPd · Grade 7Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
345-540 MPa
Higher than 41% of the catalogue
Machinability
Medium · 35
Higher than 33% of its family
Density
4.51 g/cm³
Higher than 24% of the catalogue
EN 3.7235Designación TiPdAISI/SAE Grade 7UNS R52400AMS 4900 (aprox.)ASTM B265 Grade 7 / B348 Grade 7 / B861 Grade 7AFNOR T40PdBS TA9 (aprox.)GB/T TA9GOST VT1-0Pd (aprox.)Alias Ti Gr7Alias Ti Grade 7Alias Grade 7 titaniumAlias palladium titaniumAlias titanio paladio
See recommended Vc and feed →

Indicative chemical composition (%)

Ti restoPd 0.12-0.25Fe ≤0.30O ≤0.25C ≤0.08N ≤0.03H ≤0.015

Mechanical properties

Elastic limit (Re)

≥275 MPa

Alargamiento (A%)

≥20 %

Thermal and electrical properties

Thermal conductivity

17 W/m·K

Thermal expansion

9 µm/m·K

electrical resistivity

0.48 µΩ·m

Workshop behavior

Weldability

Good

Inert atmosphere

Corrosion resistance

Higher than Grade 2 in reducing acids and chloride cracks

Fatigue resistance

Very good fatigue/weight ratio

Sensitive to surface finish

Impact resistance

Good

And retained at low temperature

Magnetic?

No

Heat treatable

No

Vc on the lathe

70–140 m/min

Carbide, medium cut

Vc in milling

70–140 m/min

Carbide, medium cut

Achievable finish (Ra)

0.8–3.2µm

Built-up edge limits very fine finishes

See recommended Vc and feed →

Recommended coolant

Abundant high pressure cooling

Whole oil or highly concentrated emulsion. Avoid chlorinated refrigerants (stress corrosion)

Chip control

Short and very hot chip, concentrated on the edge

Risk of ignition if fine buildup

Typical uses

  • Chemical equipment of maximum demand in corrosion
  • Exchangers in acidic environments

Machining notes and operator tips

Same machining behavior as Grade 2; palladium only improves chemical resistance.

  • Never stop feeding with the tool in contact; the heat concentrates and damages the edge and the part.
  • Do a single finishing pass whenever you can: going over hardens the already machined surface.
  • Keep the pass depth above the hardened layer thickness of the previous pass.

Calculate weight and cost of raw bar

Estimated weight

1.417 kg

Sources

  • Standard: ASTM B265 · Grade 7
  • Standard: ASTM B348 · Grade 7
  • Standard: ASTM B861 · Grade 7
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · R52400
  • Standard: ISO 513:2012 · S
  • Manufacturer's official website: Sandvik Coromant MC codes · S4
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz