Titanio comercialmente puro Grado 1
STitanium3.7025 · Ti99.8 · Grade 1Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.
- Strength (Rm)
- 240-370 MPa
- Higher than 24% of the catalogue
- Hardness
- ≤120 HB
- Higher than 24% of the catalogue
- Machinability
- Medium · 40
- Higher than 46% of its family
- Density
- 4.51 g/cm³
- Higher than 24% of the catalogue
Indicative chemical composition (%)
Mechanical properties
Elastic limit (Re)
≥170 MPa
Alargamiento (A%)
≥24 %
Elastic modulus (E)
103 GPa
Shear modulus (G)
39.6 GPa
Thermal and electrical properties
Thermal conductivity
17 W/m·K
Thermal expansion
9 µm/m·K
electrical resistivity
0.48 µΩ·m
Workshop behavior
Weldability
Excellent
Inert atmosphere
Corrosion resistance
Excellent
Fatigue resistance
Very good fatigue/weight ratio
Sensitive to surface finish
Impact resistance
Good
And retained at low temperature
Magnetic?
No
Heat treatable
No
Vc on the lathe
80–160 m/min
Carbide, medium cut
Vc in milling
80–160 m/min
Carbide, medium cut
Achievable finish (Ra)
0.8–3.2µm
Built-up edge limits very fine finishes
Recommended coolant
Abundant high pressure cooling
Whole oil or highly concentrated emulsion. Avoid chlorinated refrigerants (stress corrosion)
Chip control
Short and very hot chip, concentrated on the edge
Risk of ignition if fine buildup
Typical uses
- Piezas muy conformables: fuelles, chapa embutida
- Cryogenic applications
Machining notes and operator tips
The softest and most ductile grade of titanium, somewhat easier to machine than Grade 2.
- Never stop feeding with the tool in contact; the heat concentrates and damages the edge and the part.
- Do a single finishing pass whenever you can: going over hardens the already machined surface.
- Keep the pass depth above the hardened layer thickness of the previous pass.
Calculate weight and cost of raw bar
Estimated weight
1.417 kg
Sources
- Standard: ISO 5832-2 · Grade 1
- Standard: ASTM B265 · Grade 1
- Standard: ASTM B348 · Grade 1
- Standard: ASTM F67 · Grade 1
- Standard: SAE AMS 4940 / 4941
- Standard: UNS (SAE HS-1086 / ASTM DS-56) · R50250
- Standard: ISO 513:2012 · S
- Manufacturer's official website: Sandvik Coromant MC codes · S4
- Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz
Materials in the same family
Related apps
Hardness converter
Converts shop hardness scales: HRC, HRB, HRA, HRD, superficial N/T, Brinell, Vickers, Knoop, Shore HS and Rm, with a separate table for each material family. It also works out hardness from the indentation and warns you when the test is not valid.
Cutting parameters calculator
Cutting speed (Vc), rpm, feed and theoretical surface finish for turning, milling, drilling and threading by material and tool. A starting point.
Machining quote
Instant machining quote: material, machine time, setup per batch, secondary operations and margin. Free, no sign-up.