Titanio comercialmente puro Grado 2

STitanium3.7035 · Ti99.5 · Grade 2Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
345-540 MPa
Higher than 41% of the catalogue
Hardness
≤200 HB
Higher than 45% of the catalogue
Machinability
Medium · 35
Higher than 33% of its family
Density
4.51 g/cm³
Higher than 24% of the catalogue
EN 3.7035Designación Ti99.5AISI/SAE Grade 2UNS R50400JIS TB340AMS 4902 / 4941 / 4942 / 4951ASTM B265 Grade 2 / B348 Grade 2 / F67 Grade 2AFNOR T40 / T-40BS TA2 / TA3 / TP32GB/T TA2 / TA1-AGOST VT1-0 / PT-1MISO 5832-2 Grade 2Alias Ti Gr2Alias Ti Grade 2Alias Grade 2 titaniumAlias T40Alias TA2Alias VT1-0Alias commercially pure titaniumAlias titanio Grado 2Alias AMS 4902Alias ASTM B265 Grade 2
See recommended Vc and feed →

Indicative chemical composition (%)

Ti restoFe ≤0.30O ≤0.25C ≤0.08N ≤0.03H ≤0.015

Mechanical properties

Elastic limit (Re)

≥275 MPa

Alargamiento (A%)

≥20 %

Elastic modulus (E)

103 GPa

Shear modulus (G)

39.6 GPa

Thermal and electrical properties

melting point

~1668 °C

Thermal conductivity

17 W/m·K

Thermal expansion

9 µm/m·K

electrical resistivity

0.48 µΩ·m

Workshop behavior

Weldability

Good

Inert atmosphere

Corrosion resistance

Excellent

Fatigue resistance

Very good fatigue/weight ratio

Sensitive to surface finish

Impact resistance

Good

And retained at low temperature

Magnetic?

No

Heat treatable

No

Vc on the lathe

70–140 m/min

Carbide, medium cut

Vc in milling

70–140 m/min

Carbide, medium cut

Achievable finish (Ra)

0.8–3.2µm

Built-up edge limits very fine finishes

See recommended Vc and feed →

Recommended coolant

Abundant high pressure cooling

Whole oil or highly concentrated emulsion. Avoid chlorinated refrigerants (stress corrosion)

Chip control

Short and very hot chip, concentrated on the edge

Risk of ignition if fine buildup

Typical uses

  • Intercambiadores de calor
  • Non-structural implants
  • Chemical industry

Machining notes and operator tips

Low thermal conductivity: heat is concentrated on the cutting edge. Use low Vc and good pressure cooling.

  • Never stop feeding with the tool in contact; the heat concentrates and damages the edge and the part.
  • Do a single finishing pass whenever you can: going over hardens the already machined surface.
  • Keep the pass depth above the hardened layer thickness of the previous pass.

Calculate weight and cost of raw bar

Estimated weight

1.417 kg

Sources

  • Standard: ISO 5832-2 · Grade 2
  • Standard: ASTM B265 · Grade 2
  • Standard: ASTM B348 · Grade 2
  • Standard: ASTM F67 · Grade 2
  • Standard: SAE AMS 4902 / 4941
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · R50400
  • Standard: ISO 513:2012 · S
  • Manufacturer's official website: Sandvik Coromant MC codes · S4
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps