Skip to content
Back to Materials Catalog

Titanio comercialmente puro Grado 3

STitanium3.7055 · Ti99.2 · Grade 3Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
450-600 MPa
Higher than 49% of the catalogue
Hardness
≤235 HB
Higher than 62% of the catalogue
Machinability
Medium · 32
Higher than 29% of its family
Density
4.51 g/cm³
Higher than 24% of the catalogue
EN 3.7055Designación Ti99.2AISI/SAE Grade 3UNS R50550AMS 4900ASTM B265 Grade 3 / B348 Grade 3 / F67 Grade 3AFNOR T50 / T-50BS TA6 / TA7GB/T TA3GOST VT1-0 (aprox.)ISO 5832-2 Grade 3Alias Ti Gr3Alias Ti Grade 3Alias Grade 3 titaniumAlias T50Alias commercially pure titaniumAlias titanio grado 3
See recommended Vc and feed →

Indicative chemical composition (%)

Ti restoFe ≤0.30O ≤0.35C ≤0.08N ≤0.05H ≤0.015

Mechanical properties

Elastic limit (Re)

≥380 MPa

Alargamiento (A%)

≥18 %

Thermal and electrical properties

Thermal conductivity

16 W/m·K

Thermal expansion

9 µm/m·K

electrical resistivity

0.48 µΩ·m

Workshop behavior

Weldability

Good

Inert atmosphere

Corrosion resistance

Excellent

Fatigue resistance

Very good fatigue/weight ratio

Sensitive to surface finish

Impact resistance

Good

And retained at low temperature

Magnetic?

No

Heat treatable

No

Vc on the lathe

64–128 m/min

Carbide, medium cut

Vc in milling

64–128 m/min

Carbide, medium cut

Achievable finish (Ra)

0.8–3.2µm

Built-up edge limits very fine finishes

See recommended Vc and feed →

Recommended coolant

Abundant high pressure cooling

Whole oil or highly concentrated emulsion. Avoid chlorinated refrigerants (stress corrosion)

Chip control

Short and very hot chip, concentrated on the edge

Risk of ignition if fine buildup

Typical uses

  • Chemical and marine components with higher resistance than Grade 2

Machining notes and operator tips

Higher oxygen content than Grade 2: more resistant and somewhat harder to machine.

  • Never stop feeding with the tool in contact; the heat concentrates and damages the edge and the part.
  • Do a single finishing pass whenever you can: going over hardens the already machined surface.
  • Keep the pass depth above the hardened layer thickness of the previous pass.

Calculate weight and cost of raw bar

Estimated weight

1.417 kg

Sources

  • Standard: ISO 5832-2 · Grade 3
  • Standard: ASTM B265 · Grade 3
  • Standard: ASTM B348 · Grade 3
  • Standard: ASTM F67 · Grade 3
  • Standard: SAE AMS 4900
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · R50550
  • Standard: ISO 513:2012 · S
  • Manufacturer's official website: Sandvik Coromant MC codes · S4
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps