PAlloy steel1.3505 · 100Cr6 · 52100Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
690-900 (recocido) MPa
Higher than 74% of the catalogue
Hardness
58-64 HRC (templado)
Higher than 95% of the catalogue
Machinability
Medium · 35
Higher than 33% of its family
Density
7.81 g/cm³
Higher than 52% of the catalogue
EN 1.3505Designación 100Cr6DIN 100Cr6AISI/SAE 52100UNS G52986UNE F-131JIS SUJ2AMS 6440 / 6444ASTM A295 52100AFNOR 100C6 / 100Cr6BS 534A99 / EN31GB/T GCr15GOST ShKh15ISO 683-17 100Cr6Alias F131Alias F.131Alias AISI 52100Alias EN31Alias bearing steelAlias bearing steel
See recommended Vc and feed →

Indicative chemical composition (%)

C 0.93-1.05Si 0.15-0.35Mn 0.25-0.45P ≤0.025S ≤0.015Cr 1.35-1.60

Mechanical properties

Elastic modulus (E)

210 GPa

Shear modulus (G)

80.8 GPa

Thermal and electrical properties

melting point

~1430 °C

Thermal conductivity

40 W/m·K

Thermal expansion

12 µm/m·K

electrical resistivity

0.22 µΩ·m

Workshop behavior

Weldability

Not recommended

Corrosion resistance

Low

Fatigue resistance

Good after bonus

Fatigue limit ≈45-50% of Rm

Impact resistance

Good

And improves with correct quenching and tempering

Magnetic?

Yes

Heat treatable

Yes

Vc on the lathe

117–187 m/min

Carbide, medium cut

Vc in milling

117–187 m/min

Carbide, medium cut

Achievable finish (Ra)

0.8–3.2µm

See recommended Vc and feed →

Recommended coolant

High concentration soluble emulsion (8-10%) or whole oil in heavy roughing

Chip control

Continuous chip, tougher than carbon steel

Watch the chipbreaker in the quenched-and-tempered condition

Typical uses

  • Bearing races and balls
  • Precision spindles
  • Calibres

Machining notes and operator tips

Machine in the annealed condition; final quenching comes after profiling, leaving stock for grinding.

  • In the quenched-and-tempered condition, cut Vc by 15-20% versus the same steel as-supplied and use coated inserts (TiAlN).
  • Prioritise a rigid tool and good part support: it generates more cutting force than carbon steel.
  • With hardness above 300 HB, consider a softer roughing pass before finishing to avoid stressing the edge.

Calculate weight and cost of raw bar

Estimated weight

2.454 kg

Sources

  • Standard: EN ISO 683-17 · 100Cr6
  • Standard: ASTM A295 · 52100
  • Standard: SAE AMS 6440 / 6444
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · G52986
  • Standard: ISO 513:2012 · P
  • Manufacturer's official website: Sandvik Coromant MC codes · P2
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz