36CrNiMo4 Bonus Steel

PAlloy steel1.6511 · 36CrNiMo4 · 9840 (aprox.)Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
1000-1200 MPa
Higher than 87% of the catalogue
Hardness
290-340 HB
Higher than 70% of the catalogue
Machinability
Medium · 38
Higher than 41% of its family
Density
7.85 g/cm³
Higher than 53% of the catalogue
EN 1.6511Designación 36CrNiMo4DIN 36CrNiMo4AISI/SAE 9840 (aprox.)UNS G98400ASTM A29 9840 (aprox.)AFNOR 35NCD4 / 35NiCrMo4BS 816M40 (aprox.)GB/T 40CrNi / 40CrNiAGOST 40KhN / 40KhNMISO 683-2 36CrNiMo4Alias 9840Alias 35NCD4
See recommended Vc and feed →

Indicative chemical composition (%)

C 0.32-0.40Si ≤0.40Mn 0.50-0.80P ≤0.025S ≤0.035Cr 0.90-1.20Ni 0.90-1.20Mo 0.15-0.30

Mechanical properties

Elastic limit (Re)

≥800 MPa

Alargamiento (A%)

≥11 %

Elastic modulus (E)

210 GPa

Shear modulus (G)

80.8 GPa

Thermal and electrical properties

Thermal conductivity

36 W/m·K

Thermal expansion

12 µm/m·K

electrical resistivity

0.22 µΩ·m

Workshop behavior

Weldability

Difficult

Corrosion resistance

Low

Fatigue resistance

Good after bonus

Fatigue limit ≈45-50% of Rm

Impact resistance

Good

And improves with correct quenching and tempering

Magnetic?

Yes

Heat treatable

Yes

Vc on the lathe

127–203 m/min

Carbide, medium cut

Vc in milling

127–203 m/min

Carbide, medium cut

Achievable finish (Ra)

0.8–3.2µm

See recommended Vc and feed →

Recommended coolant

High concentration soluble emulsion (8-10%) or whole oil in heavy roughing

Chip control

Continuous chip, tougher than carbon steel

Watch the chipbreaker in the quenched-and-tempered condition

Typical uses

  • Medium-sized heavy-duty axles and components
  • Tooling tools

Machining notes and operator tips

Intermediate step between 42CrMo4 and 30CrNiMo8 in resistance.

  • In the quenched-and-tempered condition, cut Vc by 15-20% versus the same steel as-supplied and use coated inserts (TiAlN).
  • Prioritise a rigid tool and good part support: it generates more cutting force than carbon steel.
  • With hardness above 300 HB, consider a softer roughing pass before finishing to avoid stressing the edge.

Calculate weight and cost of raw bar

Estimated weight

2.466 kg

Sources

  • Standard: EN ISO 683-2 · 36CrNiMo4
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · G98400
  • Standard: ISO 513:2012 · P
  • Manufacturer's official website: Sandvik Coromant MC codes · P2
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps