Skip to content
Back to Materials Catalog

20MnCr5 carburizing steel

PAlloy steel1.7147 · 20MnCr5 · 5120Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
800-1100 (cemented core) MPa
Higher than 81% of the catalogue
Hardness
≤210 HB en bruto · 58-62 HRC superficie cementada
Higher than 50% of the catalogue
Machinability
Good · 55
Higher than 69% of its family
Density
7.85 g/cm³
Higher than 53% of the catalogue
EN 1.7147Designación 20MnCr5DIN 20MnCr5AISI/SAE 5120UNS G51200ASTM A29 5120AFNOR 20MC5 / 20MnCr5BS 590M20 / 590A20GB/T 20CrMn / 20CrMnMoGOST 18KhGT / 25KhGT (aprox.)ISO 683-3 20MnCr5Alias 20MC5
See recommended Vc and feed →

Indicative chemical composition (%)

C 0.17-0.22Si ≤0.40Mn 1.10-1.40P ≤0.025S ≤0.035Cr 1.00-1.30

Mechanical properties

Elastic modulus (E)

210 GPa

Shear modulus (G)

80.8 GPa

Thermal and electrical properties

Thermal conductivity

43 W/m·K

Thermal expansion

12 µm/m·K

electrical resistivity

0.22 µΩ·m

Workshop behavior

Weldability

Medium

Corrosion resistance

Low

Fatigue resistance

Good after bonus

Fatigue limit ≈45-50% of Rm

Impact resistance

Good

And improves with correct quenching and tempering

Magnetic?

Yes

Heat treatable

Yes

Vc on the lathe

183–293 m/min

Carbide, medium cut

Vc in milling

183–293 m/min

Carbide, medium cut

Achievable finish (Ra)

0.8–3.2µm

See recommended Vc and feed →

Recommended coolant

High concentration soluble emulsion (8-10%) or whole oil in heavy roughing

Chip control

Continuous chip, tougher than carbon steel

Watch the chipbreaker in the quenched-and-tempered condition

Typical uses

  • Cemented gears and pinions with a larger section than 16MnCr5

Machining notes and operator tips

Alternative to 16MnCr5 with slightly more hardenability for thicker parts.

  • In the quenched-and-tempered condition, cut Vc by 15-20% versus the same steel as-supplied and use coated inserts (TiAlN).
  • Prioritise a rigid tool and good part support: it generates more cutting force than carbon steel.
  • With hardness above 300 HB, consider a softer roughing pass before finishing to avoid stressing the edge.

Calculate weight and cost of raw bar

Estimated weight

2.466 kg

Sources

  • Standard: EN ISO 683-3 · 20MnCr5
  • Standard: ASTM A29 · 5120
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · G51200
  • Standard: ISO 513:2012 · P
  • Manufacturer's official website: Sandvik Coromant MC codes · P2
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps