Skip to content
Back to Materials Catalog

Spring steel 50CrV4

PAlloy steel1.8159 · 50CrV4 · 6150Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
1200-1450 (quenched and tempered) MPa
Higher than 94% of the catalogue
Hardness
45-50 HRC
Higher than 83% of the catalogue
Machinability
Medium · 40
Higher than 46% of its family
Density
7.85 g/cm³
Higher than 53% of the catalogue
EN 1.8159Designación 50CrV4DIN 50CrV4AISI/SAE 6150UNS G61500AMS 6448 / 6450ASTM A29 6150 / A231AFNOR 50CV4 / 51CV4BS 735A50 / 735H51GB/T 50CrVAGOST 50KhFAISO 683-14 50CrV4Alias AISI 6150Alias 50CV4Alias spring steelAlias spring steel
See recommended Vc and feed →

Indicative chemical composition (%)

C 0.47-0.55Si ≤0.40Mn 0.70-1.10P ≤0.025S ≤0.025Cr 0.90-1.20V 0.10-0.25

Mechanical properties

Elastic modulus (E)

210 GPa

Shear modulus (G)

80.8 GPa

Thermal and electrical properties

Thermal conductivity

40 W/m·K

Thermal expansion

12 µm/m·K

electrical resistivity

0.22 µΩ·m

Workshop behavior

Weldability

Difficult

Corrosion resistance

Low

Fatigue resistance

Good after bonus

Fatigue limit ≈45-50% of Rm

Impact resistance

Good

And improves with correct quenching and tempering

Magnetic?

Yes

Heat treatable

Yes

Vc on the lathe

133–213 m/min

Carbide, medium cut

Vc in milling

133–213 m/min

Carbide, medium cut

Achievable finish (Ra)

0.8–3.2µm

See recommended Vc and feed →

Recommended coolant

High concentration soluble emulsion (8-10%) or whole oil in heavy roughing

Chip control

Continuous chip, tougher than carbon steel

Watch the chipbreaker in the quenched-and-tempered condition

Typical uses

  • Springs and leaf springs
  • Herramientas manuales de alta resistencia

Machining notes and operator tips

Classic spring steel; high fatigue resistance after quenching and tempering.

  • In the quenched-and-tempered condition, cut Vc by 15-20% versus the same steel as-supplied and use coated inserts (TiAlN).
  • Prioritise a rigid tool and good part support: it generates more cutting force than carbon steel.
  • With hardness above 300 HB, consider a softer roughing pass before finishing to avoid stressing the edge.

Calculate weight and cost of raw bar

Estimated weight

2.466 kg

Sources

  • Standard: EN 10089 · 50CrV4
  • Standard: ASTM A29 · 6150
  • Standard: ASTM A231
  • Standard: SAE AMS 6448 / 6450
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · G61500
  • Standard: ISO 513:2012 · P
  • Manufacturer's official website: Sandvik Coromant MC codes · P2
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps