Skip to content
Back to Materials Catalog

Alloy steel 42CrMo4

PAlloy steel1.7225 · 42CrMo4 · 4140 / 4142Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
900-1100 (bonificado) MPa
Higher than 83% of the catalogue
Hardness
270-310 HB
Higher than 65% of the catalogue
Machinability
Medium · 45
Higher than 54% of its family
Density
7.85 g/cm³
Higher than 53% of the catalogue
EN 1.7225Designación 42CrMo4DIN 42CrMo4AISI/SAE 4140 / 4142UNS G41400UNE F-1252JIS SCM440AMS 6382 / 6529 / 6349ASTM A29 4140 / A519 4140 / A193 B7AFNOR 42CD4 / 42CrMo4BS 708M40 / 708A42 / EN19GB/T 42CrMo / 42CrMoAGOST 38KhM / 40KhMISO 683-2 42CrMo4Alias F1252Alias F.1252Alias 4140Alias 4142Alias EN19Alias 708M40Alias AISI 4140
See recommended Vc and feed →

Indicative chemical composition (%)

C 0.38-0.45Si ≤0.40Mn 0.60-0.90P ≤0.025S ≤0.035Cr 0.90-1.20Mo 0.15-0.30

Mechanical properties

Elastic limit (Re)

≥650 MPa

Alargamiento (A%)

≥12 %

Elastic modulus (E)

210 GPa

Shear modulus (G)

80.8 GPa

Thermal and electrical properties

melting point

~1416 °C

Thermal conductivity

42 W/m·K

Thermal expansion

12 µm/m·K

electrical resistivity

0.22 µΩ·m

Workshop behavior

Weldability

Medium

Preheat, risk of cold cracking

Corrosion resistance

Low

Fatigue resistance

Good after bonus

Fatigue limit ≈45-50% of Rm

Impact resistance

Good

And improves with correct quenching and tempering

Magnetic?

Yes

Heat treatable

Yes

Vc on the lathe

150–240 m/min

Carbide, medium cut

Vc in milling

150–240 m/min

Carbide, medium cut

Achievable finish (Ra)

0.8–3.2µm

See recommended Vc and feed →

Recommended coolant

High concentration soluble emulsion (8-10%) or whole oil in heavy roughing

Chip control

Continuous chip, tougher than carbon steel

Watch the chipbreaker in the quenched-and-tempered condition

Typical uses

  • Drive shafts
  • Pinions
  • Husillos
  • Tooling tools

Machining notes and operator tips

Classic quenched-and-tempered steel; in the hardened and tempered condition it needs lower Vc and coated inserts.

  • In the quenched-and-tempered condition, cut Vc by 15-20% versus the same steel as-supplied and use coated inserts (TiAlN).
  • Prioritise a rigid tool and good part support: it generates more cutting force than carbon steel.
  • With hardness above 300 HB, consider a softer roughing pass before finishing to avoid stressing the edge.

Calculate weight and cost of raw bar

Estimated weight

2.466 kg

Sources

  • Standard: EN ISO 683-2 · 42CrMo4
  • Standard: ASTM A29 · 4140
  • Standard: ASTM A519 · 4140
  • Standard: ASTM A193 · B7
  • Standard: SAE AMS 6382 / 6529
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · G41400
  • Standard: ISO 513:2012 · P
  • Manufacturer's official website: Sandvik Coromant MC codes · P2
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps