15CrNi6 carburizing steel

PAlloy steel1.5919 · 15CrNi6 · 3115 (aprox.)Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.

Strength (Rm)
900-1200 (cemented core) MPa
Higher than 87% of the catalogue
Hardness
58-62 HRC superficie cementada
Higher than 92% of the catalogue
Machinability
Medium · 45
Higher than 54% of its family
Density
7.85 g/cm³
Higher than 53% of the catalogue
EN 1.5919Designación 15CrNi6DIN 15CrNi6AISI/SAE 3115 (aprox.)UNS G31150ASTM A29 3115 (aprox.)AFNOR 16NC6 (aprox.)BS 655M13 / 655A12 (aprox.)GB/T 15CrNi6GOST 12KhN3A (aprox.)ISO 683-3 15CrNi6Alias 3115
See recommended Vc and feed →

Indicative chemical composition (%)

C 0.12-0.18Si ≤0.40Mn 0.40-0.70P ≤0.025S ≤0.035Cr 1.40-1.70Ni 1.40-1.70

Mechanical properties

Elastic modulus (E)

210 GPa

Shear modulus (G)

80.8 GPa

Thermal and electrical properties

Thermal conductivity

36 W/m·K

Thermal expansion

12 µm/m·K

electrical resistivity

0.22 µΩ·m

Workshop behavior

Weldability

Medium

Corrosion resistance

Low

Fatigue resistance

Good after bonus

Fatigue limit ≈45-50% of Rm

Impact resistance

Good

And improves with correct quenching and tempering

Magnetic?

Yes

Heat treatable

Yes

Vc on the lathe

150–240 m/min

Carbide, medium cut

Vc in milling

150–240 m/min

Carbide, medium cut

Achievable finish (Ra)

0.8–3.2µm

See recommended Vc and feed →

Recommended coolant

High concentration soluble emulsion (8-10%) or whole oil in heavy roughing

Chip control

Continuous chip, tougher than carbon steel

Watch the chipbreaker in the quenched-and-tempered condition

Typical uses

  • Engranajes de alta exigencia
  • Cemented aeronautical components

Machining notes and operator tips

Greater hardenability and core toughness than 16MnCr5; used in critical parts.

  • In the quenched-and-tempered condition, cut Vc by 15-20% versus the same steel as-supplied and use coated inserts (TiAlN).
  • Prioritise a rigid tool and good part support: it generates more cutting force than carbon steel.
  • With hardness above 300 HB, consider a softer roughing pass before finishing to avoid stressing the edge.

Calculate weight and cost of raw bar

Estimated weight

2.466 kg

Sources

  • Standard: EN ISO 683-3 · 15CrNi6
  • Standard: UNS (SAE HS-1086 / ASTM DS-56) · G31150
  • Standard: ISO 513:2012 · P
  • Manufacturer's official website: Sandvik Coromant MC codes · P2
  • Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz

Materials in the same family

See the full material catalogue

Related apps