Case hardening steel 20NiCrMo2
PAlloy steel1.6523 · 20NiCrMo2 · 8620Indicative reference data. Always check the supplier's mill certificate (3.1) before using them on critical parts.
- Strength (Rm)
- 780-1080 (cemented core) MPa
- Higher than 79% of the catalogue
- Hardness
- ≤215 HB en bruto · 58-62 HRC superficie cementada
- Higher than 52% of the catalogue
- Machinability
- Good · 55
- Higher than 69% of its family
- Density
- 7.85 g/cm³
- Higher than 53% of the catalogue
Indicative chemical composition (%)
Mechanical properties
Elastic modulus (E)
210 GPa
Shear modulus (G)
80.8 GPa
Thermal and electrical properties
Thermal conductivity
40 W/m·K
Thermal expansion
12 µm/m·K
electrical resistivity
0.22 µΩ·m
Workshop behavior
Weldability
Medium
Corrosion resistance
Low
Fatigue resistance
Good after bonus
Fatigue limit ≈45-50% of Rm
Impact resistance
Good
And improves with correct quenching and tempering
Magnetic?
Yes
Heat treatable
Yes
Vc on the lathe
183–293 m/min
Carbide, medium cut
Vc in milling
183–293 m/min
Carbide, medium cut
Achievable finish (Ra)
0.8–3.2µm
Recommended coolant
High concentration soluble emulsion (8-10%) or whole oil in heavy roughing
Chip control
Continuous chip, tougher than carbon steel
Watch the chipbreaker in the quenched-and-tempered condition
Typical uses
- Automotive gears and transmission
- Pinion shafts
- Precision case-hardened components
Machining notes and operator tips
One of the most widely used case-hardening steels worldwide (AISI 8620 is its American equivalent; in Europe it is used as an alternative to 16MnCr5).
- In the quenched-and-tempered condition, cut Vc by 15-20% versus the same steel as-supplied and use coated inserts (TiAlN).
- Prioritise a rigid tool and good part support: it generates more cutting force than carbon steel.
- With hardness above 300 HB, consider a softer roughing pass before finishing to avoid stressing the edge.
Calculate weight and cost of raw bar
Estimated weight
2.466 kg
Sources
- Standard: EN ISO 683-3 · 20NiCrMo2
- Standard: ASTM A29 · 8620
- Standard: ASTM A322 · 8620
- Standard: SAE AMS 6274 / 6276
- Standard: UNS (SAE HS-1086 / ASTM DS-56) · G86200
- Standard: ISO 513:2012 · P
- Manufacturer's official website: Sandvik Coromant MC codes · P2
- Secondary source: Sandvik Coromant Technical Guide · Vc, f, fz
Materials in the same family
Related apps
Hardness converter
Converts shop hardness scales: HRC, HRB, HRA, HRD, superficial N/T, Brinell, Vickers, Knoop, Shore HS and Rm, with a separate table for each material family. It also works out hardness from the indentation and warns you when the test is not valid.
Cutting parameters calculator
Cutting speed (Vc), rpm, feed and theoretical surface finish for turning, milling, drilling and threading by material and tool. A starting point.
Machining quote